6061 vs 6082 vs 7075 Aluminum | Quick Reference Sheet
Bookmark this quick comparison for your next engineering project!
⬛️ Tensile Strength (MPa): 7075 (572) > 6082 (340) > 6061 (310)
⬛️ Hardness (HB): 7075 (150) > 6082 (100) > 6061 (95)
⬛️ Anodize Finish: 6061 (Best) > 6082 (Good) > 7075 (Fair)
⬛️ Machinability: 6061 & 6082 (Excellent) > 7075 (Good)
⬛️ Weldability: 6061 & 6082 (Yes) | 7075 (No)