🔥 Trouble: Specimen always fractures at the grips during tensile tests?
Fracture within the grip zone makes your test results **invalid per ISO & GB standards**. Wasted samples, lost time and unreliable data — many material testing labs run into this headache.
✅ 5 Common Root Causes
🔹 Excessive clamping force: Over‑tight jaws indent soft materials and create crack origins
🔹 Mismatched grips & jaws: One‑grip‑for‑all leads to notch effect & uneven stress
🔹 Misaligned mounting: Offset specimens generate extra bending moment
🔹 Non‑standard clamping length: Improper sample cutting amplifies stress concentration
🔹 Machine mechanical deviation: Frame tilt & poor grip coaxiality cause inherent eccentricity
🛠 5 Practical Fixes
✔ Set proper clamping force: No slipping, no indentation
✔ Match jaws / liners to your test materials, replace worn jaws
✔ Install specimens: centered, vertical and aligned
✔ Re‑level machine & calibrate grip coaxiality regularly
✔ Prepare specimens strictly following standards, remove burrs & scratches
Stop invalid tests caused by grip‑end fracture. Get consistent, compliant tensile test data for your lab!